1117 Cold Finished Steel Bar
Chemical Composition
Carbon:        0.14%-0.20%
Manganese:   1.00%-1.30%
Phosphorus:   0.04% (Max)
Sulfur:        0.08%-0.013%
Properties
Tensile Strength: 69,000 psi.
Yield Strength: 58,000 psi.
Elongation in 2": 15%


*These numbers are "Typical" properties and may not be required to meet this grade. Please check with your Alro Sales Representative if physical properties are required for your application.*
 
Typical Uses
Typical applications for 1117 include:
  • Automatic Screw Machine parts
  • Carburized Parts
  • Gears
  • Pinions
  • King Pins
  • Ratchets
  • Studs
  • Cam Shafts

1117 CF Steel Bar

Alro stocks C1117 - a low carbon, high manganese steel. Machinability is improved over 1018, and case hardening is deep and uniform, supported by a tough ductile core. 1117 is a resulphurized steel with superior case hardening characteristics.
 

About 1117 Steel

1117 is a low carbon, high manganese steel. Machinability is improved over 1018 and case hardening is deep and uniform, supported by a tough ductile core. A free machining grade with improved mechanical properties suitable for carburized parts.